Numerical simulation cyclic creep effect according to uniaxial loading programs.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 711, doi. 10.1007/s11223-010-9258-5
- By:
- Publication type:
- Article
Life prediction of titanium and aluminum alloys under fretting fatigue conditions using various crack propagation criteria. Part 1. Experimental and calculation techniques.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 683, doi. 10.1007/s11223-010-9256-7
- By:
- Publication type:
- Article
Parameters of deformation mixed modes with account of crack tip curvature.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 660, doi. 10.1007/s11223-010-9254-9
- By:
- Publication type:
- Article
Computational model of the ultimate hardening of materials under high-cycle fatigue and determination of its parameters. Part 1. Description of the model.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 717, doi. 10.1007/s11223-010-9259-4
- By:
- Publication type:
- Article
U-SANS analysis of as-sintered and PEC-treated NiTi SMA produced by metal injection moulding.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 728, doi. 10.1007/s11223-010-9260-y
- By:
- Publication type:
- Article
Effect of the deposition and thickness parameters of titanium nitride (TiN) coatings on the fatigue strength.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 675, doi. 10.1007/s11223-010-9255-8
- By:
- Publication type:
- Article
Structural optimization of composite panels under strength and stability restrictions.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 631, doi. 10.1007/s11223-010-9251-z
- By:
- Publication type:
- Article
The use of master curve method for statistical re-evaluation of surveillance test data for WWER-1000 reactor pressure vessels.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 705, doi. 10.1007/s11223-010-9257-6
- By:
- Publication type:
- Article
Refinement of parameters of the model for nonlocalized damage accumulation to describe deformation of the steel 20.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 735, doi. 10.1007/s11223-010-9261-x
- By:
- Publication type:
- Article
Wirl vibrations of the drillstring bottom hole assembly.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 637, doi. 10.1007/s11223-010-9252-y
- By:
- Publication type:
- Article
Strain-life curves of steels and methods for determining the curve parameters. Part 1. Conventional methods.
- Published in:
- Strength of Materials, 2010, v. 42, n. 6, p. 647, doi. 10.1007/s11223-010-9253-x
- By:
- Publication type:
- Article