- Title
Removal of Thallium in Leaching Solution of Cadmium Residue From Zinc Hydrometallurgy.
- Authors
HUANG Zhongmin; ZHOU Yulin; CHEN Jingyang; XIONG Bangguo; YE Longgang
- Abstract
Thallium in leaching solution of cadmium residue was removed using anode slime as oxidizing agent. The effects of anode slime usage, reaction time, reaction temperature, anode slime particle size and solution pH on removal of thallium were investigated. The results show that under the conditions of anode slime usage of 10 g/L, reaction time of 60 min, reaction temperature of 70 °C, anode slime particle size of 100 -- 200 mesh, solution pH of 4, thallium removal rate reaches 94.05%. The anode slime is comprehensive utilization.