Corrosion resistances of passive films on low-Cr steel and carbon steel in simulated concrete pore solution.
- Authors
Liu, Ming; Cheng, Xuequn; Zhao, Gucheng; Li, Xiaogang; Pan, Yue
- Abstract
The passive ranges of carbon steel rebar and 3Cr steel rebar in saturated Ca(OH)2-simulated concrete pore solution with pH 12.6 were determined by means of cyclic voltammetry and potentiodynamic polarization curves. Chronopotentiometry was used to obtain steady-state conditions for the formation of passive films on rebar samples at different anodic potentials. Electrochemical impedance spectroscopy, Mott-Schottky and X-ray photoelectron spectrometer curves were employed to compare the formed passive films at different potentials. Additionally, cyclic polarization curves were used to compare the corrosion resistances of formed passive films on the two rebars in saturated Ca(OH)2-simulated concrete pore solution with different concentration of Cl−. The results show that the passive ranges of the two rebars are all between −0.15 and +0.6 V, and more stable passive films can be formed on both rebars at the anodic potential of +0.3 V. In the absence of Cl−, the stability and corrosion resistance of the passive film formed on the 3Cr rebar are better than those of CS rebar. The passive film of 3Cr steel has the relatively better pitting corrosion resistance than carbon steel in saturated Ca(OH)2-simulated concrete pore solution that contains different concentration of Cl−. Copyright © 2016 John Wiley & Sons, Ltd.
- Subjects
CARBON steel; CHRONOAMPEROMETRY; VOLTAMMETRY; X-ray photoelectron spectroscopy; PITTING corrosion; PASSIVATION; IMPEDANCE spectroscopy
- Publication
Surface & Interface Analysis: SIA, 2016, Vol 48, Issue 9, p981
- ISSN
0142-2421